AWM 3266 Cross Linked Polyethylene Electric Wire

AWM 3266 Cross Linked Polyethylene Electric Wire
AWM 3266 Cross Linked Polyethylene Electric Wire

Conductor: Bare, tinned copper
Insulator: Irradiated XL PE
Rated volt.: 300V
Test voltage: 2000V. 1Min
Rated temp.: 125℃

Application
AWM 3266 cross linked polyethylene electric wires are used very popularly in the home electric appliance, lighting, AUTO wire harness, aviation, military, instruments, plug etc.

Technical Parameters
Size Cross-section Conductor Insulation thickness Wire OD Max.
Structure OD Nominal Nominal Toler. Resist.20℃
AWG mm² No. /mm mm mm mm mm Ω/KM
26 0.128 7/0.16 0.48 0.39 1.30 ±0.10 148
24 0.206 7/0.20 0.60 0.39 1.40 ±0.10 93
22 0.324 13/0.18 0.75 0.39 1.55 ±0.10 55
21 0.412 17/0.18 0.88 0.39 1.70 ±0.10 46.9
20 0.519 21/0.18 0.96 0.39 1.75 ±0.10 34.6
10/0.254
19 0.653 26/0.18 1.10 0.39 1.90 ±0.10 29.1
18 0.823 33/0.18 1.20 0.39 2.00 ±0.10 23.2
16/0.254
17 1.040 21/0.254 1.38 0.39 2.20 ±0.10 20
16 1.310 26/0.254 1.55 0.39 2.35 ±0.10 14.6
15 1.650 33/0.254 1.75 0.39 2.55 ±0.10 11.3
14 2.080 41/0.254 1.95 0.39 2.75 ±0.10 8.96
13 2.630 52/0.254 2.19 0.39 3.00 ±0.10 7.10
12 3.310 65/0.254 2.44 0.39 3.25 ±0.20 5.64
11 4.170 83/0.254 2.74 0.39 3.55 ±0.20 4.48
10 5.261 105/0.254 3.43 0.39 4.25 ±0.20 3.55

Mechanical Properties
Tensile strength: ≥13.79N/mm2
Elongation at break of insulation: ≥300%
Min. bending radius: 7×OD
Standard: UL758, UL62, and UL1581 FT-2
Meet with RoHS, REACH rules.

Characteristics
AWM 3266 cross linked polyethylene electric wire has good performance in corrosion resistant and anti-chemical liquid, acid, alkali, excellent thermal stability. It is light weight and competitive price for customer’s choice.
We adopted good quality raw materials of PVC to assure our extruded wire can meet with strict quality control.